JPH0563525B2 - - Google Patents
Info
- Publication number
- JPH0563525B2 JPH0563525B2 JP58086309A JP8630983A JPH0563525B2 JP H0563525 B2 JPH0563525 B2 JP H0563525B2 JP 58086309 A JP58086309 A JP 58086309A JP 8630983 A JP8630983 A JP 8630983A JP H0563525 B2 JPH0563525 B2 JP H0563525B2
- Authority
- JP
- Japan
- Prior art keywords
- less
- steel
- cooling
- temperature
- steel plate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C21—METALLURGY OF IRON
- C21D—MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING
- C21D8/00—Modifying the physical properties by deformation combined with, or followed by, heat treatment
- C21D8/02—Modifying the physical properties by deformation combined with, or followed by, heat treatment during manufacturing of plates or strips
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Physics & Mathematics (AREA)
- Thermal Sciences (AREA)
- Crystallography & Structural Chemistry (AREA)
- Mechanical Engineering (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Heat Treatment Of Steel (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP8630983A JPS59211528A (ja) | 1983-05-17 | 1983-05-17 | 低降伏比非調質鋼の製造方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP8630983A JPS59211528A (ja) | 1983-05-17 | 1983-05-17 | 低降伏比非調質鋼の製造方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS59211528A JPS59211528A (ja) | 1984-11-30 |
JPH0563525B2 true JPH0563525B2 (en]) | 1993-09-10 |
Family
ID=13883229
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP8630983A Granted JPS59211528A (ja) | 1983-05-17 | 1983-05-17 | 低降伏比非調質鋼の製造方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS59211528A (en]) |
Families Citing this family (15)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6318020A (ja) * | 1986-07-11 | 1988-01-25 | Kobe Steel Ltd | 加速冷却法による低降伏比高張力鋼板の製造法 |
JPH0663027B2 (ja) * | 1986-07-11 | 1994-08-17 | 株式会社神戸製鋼所 | 加速冷却法による低降伏比高張力鋼板の製造法 |
JPS63189294A (ja) * | 1987-02-02 | 1988-08-04 | Sanyo Kokusaku Pulp Co Ltd | 複写方法 |
JPH0610303B2 (ja) * | 1987-03-10 | 1994-02-09 | 新日本製鐵株式会社 | 低降伏比非調質鋼の製造方法 |
JPH0610304B2 (ja) * | 1987-03-12 | 1994-02-09 | 新日本製鐵株式会社 | 低降伏比非調質鋼の製造方法 |
JPH0615689B2 (ja) * | 1987-05-19 | 1994-03-02 | 新日本製鐵株式会社 | 低降状比高張力鋼の製造方法 |
JPH01156422A (ja) * | 1987-12-11 | 1989-06-20 | Nippon Steel Corp | 降伏比の低い鋼材の製造法 |
JPH01156421A (ja) * | 1987-12-11 | 1989-06-20 | Nippon Steel Corp | 降伏比の低い鋼材の製造方法 |
JPH066743B2 (ja) * | 1987-12-16 | 1994-01-26 | 住友金属工業株式会社 | 高強度極厚鋼の製造方法 |
US5454883A (en) * | 1993-02-02 | 1995-10-03 | Nippon Steel Corporation | High toughness low yield ratio, high fatigue strength steel plate and process of producing same |
US5858130A (en) * | 1997-06-25 | 1999-01-12 | Bethlehem Steel Corporation | Composition and method for producing an alloy steel and a product therefrom for structural applications |
KR100480003B1 (ko) * | 1999-12-28 | 2005-03-30 | 주식회사 포스코 | 항복비가 우수한 건축구조용 tmcp후강판의 제조방법 |
JP4821181B2 (ja) * | 2005-06-24 | 2011-11-24 | Jfeスチール株式会社 | 加工性に優れた高張力鋼板の製造方法 |
JP4821182B2 (ja) * | 2005-06-24 | 2011-11-24 | Jfeスチール株式会社 | 加工性に優れた高張力鋼板の製造方法 |
CN104561771A (zh) * | 2014-12-26 | 2015-04-29 | 南阳汉冶特钢有限公司 | 一种低压缩比低合金高强度加硼厚板及其生产方法 |
Family Cites Families (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5739127A (en) * | 1980-08-21 | 1982-03-04 | Nippon Steel Corp | Strengthening treatment of steel |
-
1983
- 1983-05-17 JP JP8630983A patent/JPS59211528A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS59211528A (ja) | 1984-11-30 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JP4071906B2 (ja) | 低温靱性の優れた高張力ラインパイプ用鋼管の製造方法 | |
CN101849026A (zh) | 高温强度和低温韧性优异的焊接结构用钢及其制造方法 | |
JPH0563525B2 (en]) | ||
JP4344073B2 (ja) | 高温強度に優れた高張力鋼およびその製造方法 | |
JP5008879B2 (ja) | 強度および低温靭性の優れた高張力鋼板および高張力鋼板の製造方法 | |
JP4112733B2 (ja) | 強度および低温靭性に優れた50キロ(490MPa)ないし60キロ(588MPa)級の厚手高張力鋼板の製造方法 | |
JP5098317B2 (ja) | 高温強度と低温靭性に優れる溶接構造用鋼の製造方法 | |
JPH03211230A (ja) | 高耐食性低合金ラインパイプ用鋼の製造法 | |
KR101105113B1 (ko) | 저온인성 및 내식성이 우수한 저항복비 라인파이프용열연강판의 제조방법 | |
JP3043517B2 (ja) | 高強度熱延鋼板の製造方法 | |
JP3043519B2 (ja) | 高強度熱延鋼板の製造方法 | |
JPS642647B2 (en]) | ||
JPH02263918A (ja) | 耐hic性および耐ssc性に優れた高張力鋼板の製造法 | |
JPS6293312A (ja) | 応力除去焼鈍用高張力鋼材の製造方法 | |
JP2652538B2 (ja) | 溶接性及び低温靭性にすぐれる高強度鋼の製造方法 | |
JPS6289815A (ja) | 低温用高降伏点鋼の製造方法 | |
JPH0579728B2 (en]) | ||
JPH0247525B2 (en]) | ||
JPS6338518A (ja) | 耐水素誘起割れ性に優れた鋼板の製造方法 | |
JPH022929B2 (en]) | ||
JPH0445227A (ja) | 低降伏比鋼材の製造法 | |
JPS5828327B2 (ja) | 極めて優れた延性を有する極低炭素高張力鋼の製造方法 | |
JPS6367524B2 (en]) | ||
JPH0920921A (ja) | セパレーションを利用する高靱性鋼板の製造方法 | |
JPH06158160A (ja) | 経済性に優れた高張力調質鋼の製造方法 |